Budget-Friendly | |
Printability | |
Stiffness | |
Heat Resistance | |
Impact Strength |
Based on the properties of PETG-CF, it’s strongly recommended to consider the following tips to realize best performance:
Carbon fiber filament may wear out the nozzle; use a hardened steel nozzle to avoid abrasion.
Drying Condition:
Blast Drying Oven: 65 °C, 8h
X1 Series Heatbed: 75 - 85 °C, 12h
Build Plate & Bed Temperature: Smooth PEI Plate (60-80 °C); Textured PEI Plate (60-80 °C)
Printing Speed: < 200 mm/s
Nozzle Temperature: 240 - 270 ℃
Part Cooling Fan: 0 - 40%
Annealing: 65 - 70 ℃, 6 - 12 hours